This section provides a Resource Centre for anyone involved in designing and using stainless steel internally in Swimming Pool Buildings. Stainless steel has been used successfully in many swimming pools for applications such as:
tainless steels are widely used for pool ladders, wave machine grilles, handrails and diving board structures as well as in environmental engineering plant. When correctly selected, designed, fabricated and operated, they give generally good performance. However, there have been some instances of corrosion as a result of the particular atmospheric circumstances which can arise in indoor swimming pool buildings.