Stainless steel production increases by 16.9% 43.0 million tons in the first nine months of 2021

Brussels, 13 December 2021 – The International Stainless Steel Forum (ISSF) has released figures for the first nine months of 2021 showing that stainless steel melt shop production increased by 16.9% year–on–year to 43.0 million metric tons.