Stainless steel production decreases by 2.5% to 50.9 million tons in 2020

Brussels 15 March 2021 – The International Stainless Steel Forum (ISSF) has released figures for the full year 2020 showing that stainless steel melt shop production decreased by 2.5% year–on–year to 50.9 million metric tons.

 