Molybdenum-containing 2205 duplex stainless steel in biogas plants

Biogas plants make a valuable contribution to green energy generation: they provide electricity, heat, gas and vehicle fuel, thereby significantly reducing greenhouse gas emissions. Additionally, these plants contribute to the reduction of organic waste. Due to their exceptional corrosion resistance and strength, molybdenum-containing stainless steels have been proven to be an excellent choice for various biogas production applications.