Indian stainless steel plant starts using green hydrogen produced on-site

There has been a recent initiative by Jindal Stainless (JSL), a stainless steel plant in India, to utilize green hydrogen produced on-site using solar energy. The plant, located in Hisar, Haryana, has initiated the use of green hydrogen to reduce emissions, marking a significant step towards environmental sustainability.

Key points highlighted in the article include:

  1. Green Hydrogen Usage: JSL has commenced the utilization of green hydrogen generated on-site through an alkaline electrolyser powered by dedicated solar energy. This initiative is aimed at reducing the plant’s carbon emissions.
  2. Environmental Impact: By adopting green hydrogen, JSL expects to decrease approximately 54,000 tonnes of CO2 emissions over a span of 20 years. This underscores the significant environmental benefits associated with transitioning to sustainable energy sources.
  3. Technology and Efficiency: The facility employs an advanced energy management and control system to ensure efficient production and utilization of green hydrogen. This system enables real-time decision-making to optimize operational efficiency.
  4. Partnership and Government Support: The initiative is established in collaboration with Hygenco Green Energies, indicating a concerted effort between the private sector and renewable energy providers. Additionally, the project has garnered support from the Indian government, with the Ministry of Steel lauding the deployment of green hydrogen as a step towards a cleaner future.
  5. Future Plans: JSL aims to further scale up the use of green hydrogen across its manufacturing processes, highlighting a commitment to long-term sustainability goals. The company intends to leverage the success of this pilot project for broader implementation.
  6. Industry Implications: The development is expected to serve as an inspiration for other industry players to adopt cleaner practices and reduce their environmental footprint. This aligns with broader efforts within the iron and steel industry to transition towards greener technologies.
  7. Government Initiatives: The Indian government, through the Ministry of New & Renewable Energy (MNRE), has allocated a budget for pilot projects aimed at developing infrastructure for green hydrogen utilization in the iron and steel sector. This underscores the government’s commitment to promoting renewable energy adoption and fostering sustainable industrial practices.

Overall, the adoption of green hydrogen by JSL represents a significant milestone in India’s efforts to mitigate carbon emissions and transition towards a more sustainable future.