Intercontinental Technology Limited (ITL) is a 100% subsidiary of Amari Metals Limited, UK. Amari is a family of companies across three continents and is mainly engaged in manufacturing, stockholding, processing and distributing ferrous and non-ferrous metal alloys including aerospace grades. Amari is one of Europe’s Largest independent stockholders, processors and distributors of Aluminium, Steel, Titanium, Nickel and Copper Alloys.

ITL is a manufacturer of Copper-Nickel pipe fittings and flanges for marine, offshore and sea water systems. Since its inception in 1996 it has been manufacturing and exporting top quality Copper-Nickel fittings and flanges to marine and offshore industries across the globe with excellent track record. ITL has its manufacturing unit at Chittagong Export Processing Zone, Bangladesh, an exclusive industrial zone specified for foreign and local export based industries. The facilities that the zone provides are second to none in the sub-continent. The zone is about 2Km away from Chittagong sea port, main export-import hub of the country.

ITL mainly produces 90/10 & 70/30 Copper-Nickel butt weld, threaded pipe fittings and flanges for any sea water systems. Raw materials of the finest sourced from internationally reputed vendors are only used for manufacturing. Major grades of 90/10 & 70/30 Copper-Nickel used for production at ITL are given below.

Main Contact Details

Sector 4 Plot No. 37-39 Chittagong Export Processing Zone
South Halishahar Chittagong-4223
Bangladesh

T: 88-031-740079, 88-031-801101, 88-031-741134
E: sales@itlcepz.com

Rashedul Hasan
rashedul@itlcepz.com

Products

Services