An overview of the 200 series (high manganese) stainless steels, comparing properties with 300 series and commenting on potential applications
DD ENV 1090 Part 6 is the new fabrication and erection specification for stainless steel. It covers austenitic and duplex stainless steels used in buildings and other similar steel structures.
BS EN 10253-3 and 10253-4 are the EN standards for austenitic and duplex stainless steel butt-welding pipe fittings without and with specific inspection requirements. This article summarises the mechanical properties
BS EN 10296-2 is the EN standard for welded stainless steel tubes for general purposes. This article summarises the mechanical properties
BS EN 10297-2 is the EN standard for seamles stainless steel tubes for general purposes. This article summarises the mechanical properties
EN 10216-5 2005 is the European standard for stainless steel seamless tubes for pressure purposes. This article summarises the mechanical properties
The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.
BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 20014. Mechanical properties are specified, including proof and tensile strength, elongation and impact strength. The tensile properties only are tabulated in this article. LAST UPDATED 25th NOVEMBER 2014.
The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.