Paper originally delivered at the BSSA Conference ‘Stainless Solutions for a Sustainable Future’ held in Rotherham on 3rd April 2003. The main theme of this paper is the Deep Tunnel Sewer System and Changi Water Reprocessing Plant, currently under construction in Singapore. Stainless steels are used extensively throughout the plant that will provide a long-term sustainable future for the citizens of Singapore throughout this century. The role of stainless steels in Nuclear Reprocessing Plant, Desalination Plant and other water treatment projects is also touched briefly.