The table is intended to relate former BS, En, German and Swedish grade designations to the current EN steel numbers, AISI grades, (‘grades’ in (brackets), are not a true AISI grades), and UNS, (Unified Numbering System), numbers. The table is based on the ‘wrought’, i.e. long products, (bars etc), flat products, (plates etc.), steel numbers published in EN 10088 and related standards. Castings products use different compositions and so have their own steel numbers in EN 10283. There are however no ferritic stainless steel grades specified in either EN 10283 or BS 3100.
The ‘Composition Guide’ is intended to represent the composition only. This does not show the specified or typical compositions of commercially available steels. Specified ranges for the wrought European grades can be found in either the BS EN 10088-2 or BS EN 10088-3 tables. Most of the specified ranges for the ‘BS’ grades can be found in the BS 1449 or BS 970 tables. Direct links to tables giving the specified range is available for the grades with underlines in the table. Just click on the number.
As an alternative to scanning down the list try the ‘find’ facility on your keyboard, using the ‘Ctrl’ and ‘F’ keys together. Type in the term you are looking for in the dialog box that then appears.
These are comparisons only and cannot be assumed to be direct equivalent grades. The data given is not intended to replace that shown in individual standards to which reference should always be made.
EN (10088) | Common Names | BS (Wrought) | AISI | UNS | En | German | SS | EN(10283) | BS (Cast) | Composition Guide | ||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
. | . | . | . | . | . | . | . | . | . | C | Cr | Ni | Mo | Others |
1.4000 | – | 403S17 | 410S | S41008 | – | X6Cr13 | 2301 | – | – | 0.08x | 12 | – | – | – |
1.4002 | – | 405S17 | 405 | S40500 | – | X6CrAl13 | – | – | – | 0.08x | 12 | – | – | 0.2 Al |
1.4003 | 3Cr12 | – | – | S41050 | – | X2Cr11 | – | – | – | 0.03x | 11 | 0.5 | – | – |
1.4016 | – | 430S17 | 430 | S43000 | 60 | X6Cr17 | 2320 | – | – | 0.08x | 17 | – | – | – |
1.4113 | – | 434S17 | 434 | S43400 | – | X6CrMo17-1 | – | – | – | 0.08x | 17 | – | 1 | – |
1.4509 | 18CrCb | – | 441 | S44100 | – | – | – | – | – | 0.015x | 18 | – | – | NbandTi |
1.4510 | 430Ti | – | 439 | S43035 | – | X6CrTi17 | – | – | – | 0.05x | 17 | – | – | 0.6 Ti |
1.4511 | – | – | 430Nb | – | – | X6CrNb17 | – | – | – | 0.05x | 17 | – | – | 0.6 Nb |
1.4512 | – | 409S19 | 409 | S40900 | – | X6CrTi12 | – | – | – | 0.03x | 11 | – | – | 0.5 Ti |
1.4520 | – | – | – | – | – | X2CrTi17 | – | – | – | 0.025x | 17 | – | – | 0.5 Ti:0.015N |
1.4521 | – | – | 444 | S44400 | – | X2CrMoTi18-2 | – | – | – | 0.025x | 17 | – | 2 | 0.6 Ti |
1.4526 | – | – | 436 | S43600 | – | X2CrMoNb17-1 | – | – | – | 0.08x | 17 | – | 1.2 | 0.6 Nb |
1.4592 | – | – | – | – | – | X2CrMoTi2-4 | – | – | – | 0.025x | 28 | – | 4.0 | 0.6 Ti |
1.4605 | – | – | – | – | – | X2CrAlTi18-2 | – | – | – | 0.03x | 17 | – | – | 0.6 Ti:2.0 Al |
Note
Composition Guide figures are intended to be representative of the grade, not typical.
‘x’ indicates a maximum