The background to the publication of EN 10088 parts 1, 2 and 3 and EN 10095 is described. Part 1 covers chemical compositions and some physical properties of the European stainless steel grades. Part 2 covers flat products, i.e. sheets and plates, with their mechanical properties and replaces BS 1449 part 2 1983. Part 3 covers long products, i.e. bars and sections and replaces BS 970 part 1. EN 10095 covers Heat Resisting Steels and Nickel Alloys in all product forms. These only cover ‘general engineering’ purposes. Pressure purposes are covered by EN 10028 part 7, (flat products), and EN 10272, (long products). A summary table of standards is shown, which includes the separate dimensional tolerance standards
SSAS2.01-European Standardisation