The former BS1449 and BS970 316 type grades 316S12, 316S16, 316S11, 316S13, 316S31 and 316S33 are compared and matched to the current EN steel number grades. Composition ranges for the ?BS? grades are given. For atmospheric exposure service conditions, except in extreme marine environments, the substitution of either: -316S11, (1.4404), for 316S12 or 316S31 (1.4401) for 316S16 should give satisfactory corrosion resistance, depending on design and finishing techniques.
SSAS2.23-Comparison of 316S12 & S16 with 316S11,13,31 & 33