  1. Ambient temperature mechanical properties for BS EN 10253-3 and 10253-4 for stainless steel butt weld fittings

    BS EN 10253-3 and 10253-4 are the EN standards for austenitic and duplex stainless steel butt-welding pipe fittings without and with specific inspection requirements. This article summarises the mechanical properties

  2. Ambient temperature mechanical properties for EN 10216-5 for stainless steel seamless tubes for pressure purposes

    EN 10216-5 2005 is the European standard for stainless steel seamless tubes for pressure purposes. This article summarises the mechanical properties

  3. Ambient temperature mechanical properties of austenitic stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.

  4. Ambient temperature mechanical properties of austenitic stainless steel flat products to BS EN 10088-2

    BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 20014. Mechanical properties are specified, including proof and tensile strength, elongation and impact strength. The tensile properties only are tabulated in this article. LAST UPDATED 25th NOVEMBER 2014.

  5. Ambient temperature mechanical properties of austenitic stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.

  6. Ambient temperature mechanical properties of austenitic-ferritic (duplex) stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic-ferritic stainless steels.

  7. Ambient temperature mechanical properties of austenitic-ferritic (duplex) stainless steel flat products to BS EN 10088-2

    The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified, including proof and tensile strength, elongation and impact strength. The tensile properties only are tabulated in this article. LAST UPDATED 25th NOVEMBER 2014

  8. Ambient temperature mechanical properties of austenitic-ferritic (duplex) stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for austenitic-ferritic (duplex) stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given are proof strength, tensile strength, elongation and hardness.

  9. Ambient temperature mechanical properties of cold worked wire to EN 10088-3

    EN 10088-3 is the European Standard for stainless steel long products. It includes a provision for wire in the cold worked condition. Although this is not strictly for spring wire (which is EN 10270-3), the properties shown in Table 18 are such that springs could be made from material in this condition

  10. Ambient temperature mechanical properties of stainless steels to BS EN 10269

    BS EN 10269 is the material standard for stainless and heat-resisting steels, a selection of low alloy steels and some nickel alloys for fasteners. The ambient temperature mechanical properties shown in this article include 0.2% proof strength, tensile strength, elongation, reduction in area and impact (charpy) strength in the finally heat treated condition. Specified hardness levels for the steels for subsequent quenching and tempering (1.4923 1.4938 and 1.4913) in their delivery condition are also included.