BS EN 10253-3 and 10253-4 are the EN standards for austenitic and duplex stainless steel butt-welding pipe fittings without and with specific inspection requirements. This article summarises the mechanical properties
BS EN 10297-2 is the EN standard for seamless stainless steel tubes for general purposes. This article summarises the mechanical properties
EN 10216-5 2005 is the European standard for stainless steel seamless tubes for pressure purposes. This article summarises the mechanical properties
The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.
BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 20014. Mechanical properties are specified, including proof and tensile strength, elongation and impact strength. The tensile properties only are tabulated in this article. LAST UPDATED 25th NOVEMBER 2014.
The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.
The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic-ferritic stainless steels.
The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified, including proof and tensile strength, elongation and impact strength. The tensile properties only are tabulated in this article. LAST UPDATED 25th NOVEMBER 2014
The BS EN 10088-3 standard gives the mechanical properties for austenitic-ferritic (duplex) stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given are proof strength, tensile strength, elongation and hardness.
EN 10088-3 is the European Standard for stainless steel long products. It includes a provision for wire in the cold worked condition. Although this is not strictly for spring wire, (which is EN 10270-3), the properties shown in Table 18 are such that springs could be made from material in this condition