  1. Chemical composition of stainless steel castings to BS EN 10283

    BS EN 10283 is the material standard for stainless steel castings for corrosion resisting purposes. The chemical composition of stainless steel grades covered in the this standard include 1.4011, 1.4008, 1.4317, 1.4405, 1.4411, 1.4525, 1.4309, 1.4308, 1.4552, 1.4409, 1.4408, 1.4581, 1.4412, 1.4446, 1.4458, 1.4527, 1.4584, 1.4416, 1.4587, 1.4588, 1.4593, 1.4347, 1.4470, 1.4468, 1.4517, 1.4417, and 1.4469.

  2. Chemical composition of stainless steels to BS 3100

    BS 3100 is the material standard for stainless steel castings for corrosion resisting purposes. The chemical composition of stainless steel grades covered in the this standard include 410C21, 420C28, 420C29, 425C12, 425C11, 302C25, 304C12, 304C15, 347C17, 316C12, 316C16, 317C16, 318C17, 332C11, 332C13, 332C15, 420C24, 452C11, 452C12, 302C35, 309C30, 309C40, 310C45, 311C11, 330C12, 331C60, 334C11, 309C32, 309C35, 310C40, 330C11, 331C40

  3. Chemical compositions of ACI stainless and heat resisting steel castings grades

    ASTM standards A297, A351, A743, A744 and A890 specify castings for corrosion and heat-resisting service. These include stainless steels and some nickel based alloys. The grade designations used in these standards are those originally developed by the ACI, the Alloy Casting Institute. (Now the Steel Founder’s Society of America). The chemical composition of stainless steel grades covered by these standards include ACI grade designations CA6N, CA6NM, CA15, CA15M, CA28MWV, CA40, CA40F, CB6, CB30, CB7Cu-1, CB7Cu-2, CC50, CD3MCuN, CD3MN, CD3MWCuN, CD4MCu, CD6MN, CE20N, CE3MN, CE30, CE8MN, CF3, CF8, CF8C, CF20, CF3M, CF3MN, CF8M, CF8C, CF10, CF10M, CF10MC, CF10SMnN, CF16F, CF16FA, CG6MMN, CG3M, CG8M, CG12, CH8, CH10, CH20, CK20, CK3MCuN, CK35MN, CN3M, CN3MN, CN7M, CN7MSCT15C, HC, HD, HE, HF, HH, HI, HK, HK30, HK40, HL, HN, HP, HT, HT30, HU, HW, HX. Duplex castings grades, 1A, 1B, 1C, 2A, 3A, 4A, 5A, 6A, are also listed and cross references to wrought AISI grades, 410, 420, 304L, 304, 347, 302, 316L, 316LN, 316, 317, 317L, 309, 310, made. Common grade names are also cross referenced and include, 17/4PH, 15/5PH, 2205, Zeron 100, Alloy 958, Escoloy, 254SMO, and AL-6XN

  4. Chemical compositions of stainless steels to BS 3146-2

    BS 3146-2 is the material standard for castings, to be made by the investment, (or lost wax), process and includes some stainless steels. The chemical composition of stainless steel grades covered in the this standard include, ANC1-A, ANC1-B, ANC1-C, ANC2, ANC3-A, ANC3-B, ANC4-A, ANC4-B, ANC4C, ANC5-A, ANC5-B, ANC5-C, ANC6-A, ANC6-B, ANC6-C, ANC20A, ANC20B, and ANC21