Members Area
T: +44 (0)114 551 8170
E: ssas@bssa.org.uk

Availability of Stainless Steel Grades

Availability of Stainless Steel Products

The tables below give an indication of the availability of stainless steel flat and long products. The intention is to give designers and specifiers some idea of how easy it will be to source their choice of grade and product form. The information has been created as a response to enquiries for rare grades which are difficult to source in small quantities.

Comments are invited on the tables. It is likely with such a large amount of information that there are some differences of opinion about the availability of some grades. If you want to make a comment on this table please email to ssas@bssa.org.uk.

Availability of Flat Products Grades from EN 10088-2

The table below contains all grades listed in EN 10088-2. The meaning of the availability scores is:

1 – Readily available from any recognised stainless steel stockholder

2 – Available from a significant number of specialist stainless steel stockholders

3 – Available from a limited number of suppliers

4 – Available only from stainless steel mills if sufficient quantity required

5 – Not practically available

N/A – Not applicable – Indicates that the grade is not intended to be made in that product form. For example, most ferritic grades would not be made as plate.

EN Designation Alternative Designations  Availability
Steel name Steel number AISI UNS Other US BS Generic/Brand Plate Sheet
Ferritic stainless steels – standard grades
X2CrNi12 1.4003 S40977 3CR12 2 2
X2CrTi12 1.4512 409 S40900 409S19 N/A 2
X6CrNiTi12 1.4516 N/A 4
X6Cr13 1.4000 410S S41008 403S17 3 3
X6CrAl13 1.4002 405 S40500 405S17 4 4
X6Cr17 1.4016 430 S43000 430S17 N/A 1
X3CrTi17 1.4510 439 S43035 N/A 2
X3CrNb17 1.4511 430Nb N/A 4
X6CrMo17-1 1.4113 434 S43400 434S17 N/A 4
X2CrMoTi18-2 1.4521 444 S44400 N/A 3
Ferritic stainless steels – special grades
X2CrTi17 1.4520 N/A 4
X1CrNb15 1.4595 N/A 4
X2CrMoTi17-1 1.4513 N/A 4
X6CrNi17-1 1.4017 N/A 4
X5CrNiMoTi15-2 1.4589 S42035 N/A 4
X6CrMoNb17-1 1.4526 436 S43600 N/A 3
X2CrNbZr17 1.4590 N/A 4
X2CrTiNb18 1.4509 441 S43932 18CrCb N/A 2
X2CrMoTi29-4 1.4592 S44700 29-4 N/A 4
X2CrMnNiTi12 1.4600 N/A 3
X2CrSiTi15 1.4630 N/A 3
X2CrAlSiNb18 1.4634 N/A 3
X2CrNbTi20 1.4607 N/A 3
X2CrTi21 1.4611 N/A 3
X2CrNbCu21 1.4621 N/A 3
X2CrTi24 1.4613 N/A 3
Ferritic stainless steels – heat resisting grades
X10CrAlSi7 1.4713 3 3
X10CrAlSi13 1.4724 3 3
X10CrAlSi18 1.4742 3 3
X18CrN28 1.4749 446 3 3
X10CrAlSi25 1.4762 3 3
Martensitic stainless steels – standard grades
X12Cr13 1.4006 410 S41000 410S21 3 3
X15Cr13 1.4024 420 S42000 3 3
X20Cr13 1.4021 420 S42000 420S29 3 3
X30Cr13 1.4028 420 S42000 420S45 3 3
X39Cr13 1.4031 420 S42000 420S45 3 3
X46Cr13 1.4034 420 S42000 3 3
X38CrMo14 1.4419 5 5
X55CrMo14 1.4110 5 5
X50CrMoV15 1.4116 4 4
X39CrMo17-1 1.4122 5 5
X3CrNiMo13-4 1.4313 S41500 F6NM 3 3
X4CrNiMo16-5-1 1.4418 248 SV 3 3
Martensitic and precipitation-hardening steels – special grades
X1CrNiMoCu12-5-2 1.4422 5 5
X1CrNiMoCu12-7-3 1.4423 5 5
X5CrNiCuNb16-4 1.4542 S17400 17-4 PH 3 3
X7CrNiAl17-7 1.4568 S17700 17-7 PH N/A 2
Austenitic stainless steels – standard grades
X10CrNi18-8 1.4310 301 S30100 301S21 N/A 2
X2CrNiN18-7 1.4318 301LN S30153 N/A 3
X2CrNi18-9 1.4307 304L S30403 304S11 1 1
X2CrNi19-11 1.4306 304L S30403 4 4
X2CrNiN18-10 1.4311 304LN S30453 304S51 3 4
X5CrNi18-10 1.4301 304 S30400 304S15 1 1
X8CrNiS18-9 1.4305 303 S30300 303S31 3 N/A
X6CrNiTi18-10 1.4541 321 S32100 321S31 2 2
X4CrNi18-12 1.4303 305 S30500 305S19 N/A 4
X2CrNiMo17-12-2 1.4404 316L S31603 316S11 1 1
X2CrNiMoN17-11-2 1.4406 316LN S31653 316S61 4 4
X5CrNiMo17-12-2 1.4401 316 S31600 316S31 1 1
X6CrNiMoTi17-12-2 1.4571 316Ti S31635 320S31 3 3
X2CrNiMo17-12-3 1.4432 316L S31603 316S13 2 3
X2CrNiMo18-14-3 1.4435 316L S31603 316S13 4 4
X2CrNiMoN17-13-5 1.4439 317LMN 4 4
X1NiCrMoCu25-20-5 1.4539 N08904 904S13  904L 3 3
Austenitic stainless steels – special grades
X5CrNi17-7 1.4319 4 4
X5CrNiN19-9 1.4315 4 4
X1CrNi25-21 1.4335 310L 4 4
X6CrNiNb18-10 1.4550 347 S34700 347S31 4 3
X1CrNiMoN25-22-2 1.4466 310MoLN S31050 4 4
X6CrNiMoNb17-12-2 1.4580 5 5
X2CrNiMoN17-3-3 1.4429 316LN S31653 4 4
X3CrNiMo17-13-3 1.4436 316 S31600 316S33 3 3
X2CrNiMoN18-12-4 1.4434 317LN S31753 4 4
X2CrNiMo18-15-4 1.4438 317L 317S12 4 4
X1CrNiMoCuN24-22-8 1.4652 4 4
X1CrNiSi18-15-4 1.4361 4 4
X11CrNiMnN19-8-6 1.4369 4 3
X12CrMnNiN17-7-5 1.4372 201 S20100 4 3
X2CrMnNiN17-7-5 1.4371 201L S20103 4 3
X12CrMnNiN18-9-5 1.4373 202 S20200 4 3
X9CrMnCuNB17-8-3 1.4597 204Cu S20430 N/A 3
X1NiCrMo31-27-4 1.4563 N08028 Sanicro 28 4 4
X1CrNiMoCuN25-25-5 1.4537 5 5
X1CrNiMoCuN20-18-7 1.4547 S31254 F44 254SMO 3 3
X1CrNiMoCuNW24-22-6 1.4659 4 4
X1NiCrMoCuN25-20-7 1.4529 N08925 1925hMo 3 3
X2CrNiMnMoN25-18-6-5 1.4565 3 N/A
X9CrMnNiCu 17-8-5-2 1.4618 N/A 3
X2CrNiMnMoNNb21-16-5-3 1.3964 XM-19 3 N/A
X8CrMnNi19–6-3 1.4376 3 3
X5CrNiCu19–6-2 1.4640 3 3
X6CrMnNiCuN18–12–4-2 1.4646 3 3
Austenitic stainless steels – heat resisting grades
X8CrNiTi18-10 1.4878 321 S32100 3 3
X15CrNiSi20-12 1.4828 3 3
X9CrNiSiNCe21-11-2 1.4835 S30815 253 MA 3 3
X12CrNi23-13 1.4833 309 S30900 309S24 3 3
X8CrNi25-21 1.4845 310S S31000 310S24 2 2
X15CrNiSi25-21 1.4841 314 S31400 4 4
X6CrNiSiNCe19-10 1.4818 S30415 153 MA 4 4
X10NiCrSi35-19 1.4886 330 3 3
Austenitic stainless steels – creep resisting grades
X6CrNi18-10 1.4948 304H S30409 304S51 3 4
X6CrNiMoB17-12-2 1.4919 316H S31635 316S51 3 4
Austenitic-ferritic stainless steels-standard grades
X2CrNiN22-2 1.4062 S32202 DX 2202 3 3
X2CrMnNiN21-5-1 1.4162 S32101 2101 LDX 3 3
X2CrNiN23-4 1.4362 S32304 2304 3 3
X2CrNiMnMoCuN24–4-3–2 1.4662 2404 LDX 3 3
X2CrMnNiMoN21–5-3 1.4482 3 3
X2CrNiMoN12-5-3 1.4462 S31803/

S32205

 F51 2205 2 2
Austenitic-ferritic stainless steels-special grades
X2CrNiCuN23-4 1.4655 5 5
X2CrNiMoN29-7-2 1.4477 5 5
X2CrNiMoCuN25-6-3 1.4507  F61 Ferrinox 255 3 3
X2CrNiMoN25-7-4 1.4410 S32750  F53 2507 2 3
X2CrNiMoCuWN25-7-4 1.4501 S32760  F55 Zeron 100 2 3
X2CrNiMoSi18-5-3 1.4424 5 5

Availability of Long Products Grades from EN 10088-3

The table below contains all grades listed in EN 10088-3. The meaning of the availability scores is:

1 – Readily available from any recognised stainless steel stockholder

2 – Available from a significant number of specialist stainless steel stockholders

3 – Available from a limited number of suppliers

4 – Available only from stainless steel mills if sufficient quantity required

5 – Not practically available

N/A – Not applicable – Indicates that the grade is not intended to be made in that product form. For example, most ferritic grades would not be made as plate.

 

The table below contains all grades listed in EN 10088-3. In addition, there are some grades not in the current edition but which are expected to be in future editions. Some heat resisting steels from EN 10095 and creep resisting steels from EN 10302 are also included.

EN Designation  Alternative designation Availability
Steel name Steel number AISI UNS Other US BS Generic/Brand Bar Wire
Ferritic stainless steels-standard grades
X2CrNi12 1.4003 S40977 3 4
X6Cr13 1.4000 410S S41008 403S17 3 3
X6Cr17 1.4016 430 S43000 430S17 2 2
X6CrMoS17 1.4105 2 2
X6CrMo17-1 1.4113 434 S43400 3 3
Ferritic stainless steels-special grades
X2CrTi17 1.4520 4 4
X3CrNb17 1.4511 4 4
X2CrMoTiS18-2 4 1.4523 4 4
X6CrMoNb17-1 1.4526 436 S43600 4 4
X2CrTiNb18 1.4509 441 S43932 18CrCb 4 4
X2CrTi21 1.4611 3 3
X2CrNbCu21 1.4621 3 3
X2CrTi24 1.4613 3 3
Ferritic stainless stees – Heat resisting grades
X10CrAlSi7 1.4713 3 3
X10CrAlSi18 1.4742 4 4
X10CrAlSi25 1.4762 4 4
Martensitic stainless steels-standard grades
X12Cr13 1.4006 410 S41000 2 2
X12CrS13 1.4005 416 S41600 2 2
X20Cr13 1.4021 420 S42000 420S29 2 2
X30Cr13 1.4028 420 S42000 420S45 2 2
X39Cr13 1.4031 420 S42000 420S45 3 3
X46Cr13 1.4034 420 S42000 3 3
X38CrMo14 1.4419 4 4
X50CrMoV15 1.4116 3 3
X55CrMo14 1.4110 4 4
X14CrMoS17 1.4104 2 2
X39CrMo17-1 1.4122 2 N/A
X17CrNi16-2 1.4057 431 S43100 431S29 1 N/A
X3CrNiMo13-4 1.4313 S41500 F6NM 3 N/A
X4CrNiMo16-5-1 1.4418 248SV 3 N/A
Martensitic stainless steels-special grades
X29CrS13 1.4029 4 4
X46CrS13 1.4035 4 4
X70CrMo15 1.4109 3 4
X40CrMoVN16-2 1.4123 4 4
X105CrMo17 1.4125 440C S44004 3 N/A
X90CrMoV18 1.4112 440B S44003 3 N/A
X2CrNiMoV13-5-2 1.4415 4 4
X53CrSiMoVN16-2 1.4150 3 3
Martensitic stainless steels-creep resisting grades
X20CrMoV11-1 1.4922 3 N/A
X22CrMoV12-1 1.4923 3 N/A
Precipitation hardening stainless steels-standard grades
X5CrNiCuNb16-4 1.4542 S17400 17-4 PH 2 3
X7CrNiAl17-7 1.4568 S17700 17-7 PH N/A 3
X5CrNiMoCuNb14-5 1.4594 FV 520B 3 N/A
Precipitation hardening stainless steels-special grades
X1CrNiMoAlTi12-9-2 1.4530 4 N/A
X1CrNiMoAlTi12-10-2 1.4596 4 N/A
X5NiCrTiMoVB25-12-2 1.4606 4 N/A
X1CrNiMoAlTi12-11-2 1.4612 3 3
Austenitic stainless steels-standard grades
X10CrNi18-8 1.4310 301 S30100 301S21 N/A 1
X2CrNi18-9 1.4307 304L S30403 304S11 1 1
X2CrNi19-11 1.4306 304L S30403 304S11 3 3
X2CrNiN18-10 1.4311 304LN S30453 304S61 3 3
X5CrNi18-10 1.4301 304 S30400 304S31 1 1
X8CrNiS18-9 1.4305 303 S30300 303S31 1 1
X6CrNiTi18-10 1.4541 321 S32100 321S31 2 2
X4CrNi18-12 1.4303 305 S30500 4 4
X2CrNiMo17-12-2 1.4404 S31603 316S11 1 1
X2CrNiMoN17-11-2 1.4406 316LN S31653 4 4
X5CrMo17-12-2 1.4401 316 S31600 316S31 1 1
X6CrNiMoTi17-12-2 1.4571 316Ti S31635 320S31 2 2
X2CrNiMo17-12-3 1.4432 316L S31603 316S13 4 4
X2CrNiMoN17-13-3 1.4429 316LN S31653 3 4
X3CrNiMo17-13-3 1.4436 316 S31600 316S33 3 3
X2CrNiMo18-14-3 1.4435 316L S31603 3 3
X2CrNiMoN17-13-5 1.4439 317LMN S31726 4 4
X6CrNiCuS18-9-2 1.4570 3 3
X3CrNiCu18-9-4 1.4567 304Cu S30430 394S17 2 2
X1NiCrMoCu25-20-5 1.4539 904L N09804 904S13 2 2
Austenitic stainless steels-special grades
X5CrNi17-7 1.4319 302 S30200 302S25 4 2
X9CrNi18-9 1.4325 4 4
X5CrNiN19-9 1.4315 304N S30451 4 4
X6CrNiNb18-10 1.4550 347 S34700 347S31 3 4
X1CrNiMoN25-22-2 1.4466 310MoLN S31050 4 4
X6CrNiMoNb17-12-2 1.4580 316Cb S31640 4 4
X2CrNiMo18-15-4 1.4438 317L S31703 317S12 4 4
X1CrNiMoCuN24-22-8 1.4652 S32654 654SMO 4 4
X1CrNiSi18-15-4 1.4361 306 S30600 4 4
X11CrNiMnN19-8-6 1.4369 4 4
X12CrMnNiN17-7-5 1.4372 201 S20100 3 3
X8CrMnNiN18-9-5 1.4374 4 4
X8CrMnCuNB17-8-3 1.4597 S20430 3 3
X3CrNiCu19-9-2 1.4560 4 4
X3CrNiCuMo17-11-3-2 1.4578 4 4
X1NiCrMoCu31-27-4 1.4563 N08028 Sanicro 28 3 3
X1CrNiMoCuN25-25-5 1.4537 N08932 4 4
X1CrNiMoCuN20-18-7 4 1.4547 S31254 254 SMO 3 3
X2CrNiMoCuS17-10-2 1.4598 3 4
X1CrNiMoCuNW24-22-6 1.4659  S31266 4 4
X1NiCrMoCuN25-20-7 1.4529 N08925 1925hMo 3 3
X2CrNiMnMoN25-18-6-5 1.4565 S34565 3 4
X2CrNiMnmoNNb21-16-5-3 1.3964 S20910 Nitronic 50 3 3
S21800 Nitronic 60 3 3
X3CrMnNiCu15-8-5-3 1.4615 3 3
X13MnNiN18-13-2 1.4020 3 3
X6CrMnNiN18-3-3 1.4378 3 3
X6CrMnNiCuN18-12-4-2 1.4646 3 3
Austenitic stainless steels – Heat resisting steels
X6CrNiSiNCe19-10 1.4818 S30415 4 4
X15CrNiSi20-12 1.4828 309Si 3 3
X12CrNi23-13 1.4833 309 S30900 309S16 3 3
X9CrNiSiNCe21-11-2 1.4835 S30815 253 MA 3 3
X8CrNi25-21 1.4845 310S S31008 310S31 2 2
X15CrNiSi25-21 1.4841 314 S31400 2 2
X12NiCrSi35-16 1.4864 4 3
X10NiCrSi35-19 1.4886 330 N08330 3 3
Austenitic stainless steels – Creep resisting grades
X6CrNiMoB17-12-2 1.4919 316H S31609 4 4
X6CrNi18-10 1.4948 304H S30409 3 3
X6NiCrTiMoVB25-15-2 1.4980 S66286 A286 3 4
Austenitic-ferritic stainless steels-Standard grades
X2CrNiN22-2 1.4062 S32202 DX 2202 3 3
X2CrMnNiN21-5-1 1.4162 S32101 2101 LDX 2 2
X3CrNiMoN27-5-2 1.4460 329 S31260 3 N/A
X2CrNiMoN22-5-3 1.4462 S31803/

S32205

2205 2 2
Austenitic-ferritic stainless steels-special grades
X2CrNiN23-4 1.4362 S32304 2304 3 3
X2CrNiMoN29-7-2 4 1.4477 4 4
X2CrNiMoCuN25-6-3 1.4507 S32550 Ferrinox 255 2 2
X2CrNiMoN25-7-4 4 1.4410 S32750 2507 2 2
X2CrNiMoCuWN25-7-4 1.4501 S32760 Zeron 100 2 3
X2CrNiMoSi18-5-3 1.4424 S31500 4 4
X2CrMnNiMoN21-5-3 1.4482 3 3
X2CrNiMnMoCuN24-4-3-2 1.4662 2404 LDX 3 3
X2CrCuNiN23-2-2 1.4669 3 3

top