The table shows current standards only. ASTM standards are reviewed each year and the status updated, even if no changes have been made to the standard. The original and current year of issue is not therefore shown on the table.
Use the ‘Ctrl’ and ‘F’ keys to ‘find’ the standard you are looking for.
Std Number | Title |
---|---|
General | |
ASTM A450 | Specification for General Requirements for Carbon, Ferritic Alloy, and Austenitic Alloy Steel Tubes |
ASTM A480 | Specification for General Requirements for Flat-Rolled Stainless And Heat-Resisting Steel Plate, Sheet and Strip |
ASTM A484 | Specification for General Requirements for Stainless Steel Bars, Billets, and Forgings |
ASTM A555 | Specification for General Requirements for Stainless Steel Wire and Wire Rods |
ASTM A999 | Specification for General Requirements for Alloy and Stainless Steel Pipe |
ASTM A1016 | Specification for General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel and Stainless Steel Tubes |
Flat Products | |
ASTM A167 | Specification for Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet and Strip |
ASTM A176 | Specification for Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip |
ASTM A666 | Specification For Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate and Flat Bar |
ASTM A693 | Specification for Precipitation-Hardening Stainless And Heat-Resisting Steel Plate, Sheet and Strip |
Long Products | |
ASTM A276 | Specification for Stainless Steel Bars and Shapes |
ASTM A314 | Specification for Stainless Steel Billets and Bars for Forging |
ASTM A493 | Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging |
ASTM A564 | Specification for Hot-Rolled And Cold-Finished Age-Hardening Stainless Steel Bars and Shapes |
ASTM A565 | Specification for Martensitic Stainless Steel Bars, Forgings, and Forging Stock for High Temperature Service |
ASTM A582 | Specification for Free Machining Stainless Steel Bars |
Tubes & Pipes | |
ASTM A182 | Specification for Forged or Rolled Alloy-Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service |
ASTM A268 | Specification for Seamless and Welded Ferritic Stainless Steel Tubing for General Service |
ASTM A269 | Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service |
ASTM A312 | Seamless and Welded Austenitic Stainless Steel Pipe |
ASTM A358 | Electric Fusion Welded Austenitic Chromium Nickel Alloy Steel Pipe for High Temperature Service |
ASTM A403 | Specification for Wrought Austenitic Stainless Steel Piping Fittings |
ASTM A409 | Specification for Welded Large Diameter Austenitic Steel Pipe for Corrosive or High Temperature Service |
ASTM A511 | Specification for Seamless Stainless Steel Mechanical Tubing |
ASTM A554 | Specification for Welded Stainless Steel Mechanical Tubing |
ASTM A632 | Specification for Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service |
ASTM A731 | Specification for Seamless and Welded Ferritic Stainless Steel Pipe |
ASTM A789 | Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Tubing for General Service |
ASTM A790 | Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe |
ASTM A813 | Specification for Single or Double Welded Austenitic Stainless Steel Pipe |
ASTM A814 | Specification for Cold Worked Welded Austenitic Stainless Steel Pipe |
Forgings | |
ASTM A473 | Specification for Stainless Steel Forgings |
ASTM A705 | Specification for Age Hardening Stainless and Heat Resisting Steel Forgings |
Castings | |
ASTM A297 | Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat-Resistant for General Application |
ASTM A743 | Standard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application |
ASTM A744 | Standard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service |
ASTM A890 | Standard Specification for castings, iron-chromium-nickel-molybdenum corrosion-resistant, duplex (austenitic/ferritic) for general application |