6d. Chemical composition of valve steels to BS EN 10090

Introduction

 

As an alternative to scanning down the list try the ‘find’ facility on your keyboard, using the ‘Ctrl’ and ‘F’ keys together. Type in the term you are looking for in the dialog box that then appears.

The data given is not intended to replace that shown in individual standards to which reference should always be made.

BS EN 10090 chemical composition tables

Designation Chemical composition (% by mass – max unless stated)
Steel name Steel number C Si Mn P S Cr Mo Ni Others
Martensitic steels
X45CrSi9-3 1.4718 0.40/0.50 2.70/3.30 0.60 0.040 0.030 8.00/10.00 0.50
X40CrSiMo10-2 1.4731 0.35/0.45 2.00/3.00 0.80 0.040 0.030 9.50/11.50 0.80/1.30 0.50
X85CrMoV18-2 1.4748 0.80/0.90 1.00 1.50 0.040 0.030 16.50/18.50 2.00/2.50 V:0.30/0.60
Austenitic steels
X55CrMnNiN20-8 1.4875 0.50/0.60 0.25 7.00/10.00 0.045 0.030 19.50/21.50 1.50/2.75 N:0.20/0.40
X53CrMnNiN21-9 1.4871 0.48/0.58 0.25 8.00/10.00 0.045 0.030 20.00/22.00 3.25/4.50 N:0.35/0.50
X50CrMnNiNbN21-9 1.4882 0.45/0.55 0.45 8.00/10.00 0.045 0.030 20.00/22.00 3.50/5.50 W:0.80/1.50 Nb+Ta:1.80/2.50 N:0.40/0.60
X53CrMnNiNbN21-9 1.4870 0.48/0.58 0.45 8.00/10.00 0.045 0.030 20.00/22.00 3.25/4.50 Nb+Ta:2.00/3.00 N:0.40/0.60 C+N:0.90 min
X33CrNiMnN23-8 1.4866 0.28/0.38 0.50/1.00 1.50/3.50 0.045 0.030 22.00/24.00 0.50 7.00/9.000 W:0.50 N:0.25/0.35