Std Number Title
General
ASTM A450 Specification for General Requirements for Carbon, Ferritic Alloy, and Austenitic Alloy Steel Tubes
ASTM A480 Specification for General Requirements for Flat-Rolled Stainless And Heat-Resisting Steel Plate, Sheet and Strip
ASTM A484 Specification for General Requirements for Stainless Steel Bars, Billets, and Forgings
ASTM A555 Specification for General Requirements for Stainless Steel Wire and Wire Rods
ASTM A999 Specification for General Requirements for Alloy and Stainless Steel Pipe
ASTM A1016 Specification for General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel and Stainless Steel Tubes
Flat Products
ASTM A167 Specification for Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet and Strip
ASTM A176 Specification for Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip
ASTM A666 Specification For Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate and Flat Bar
ASTM A693 Specification for Precipitation-Hardening Stainless And Heat-Resisting Steel Plate, Sheet and Strip
Long Products
ASTM A276 Specification for Stainless Steel Bars and Shapes
ASTM A314 Specification for Stainless Steel Billets and Bars for Forging
ASTM A493 Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
ASTM A564 Specification for Hot-Rolled And Cold-Finished Age-Hardening Stainless Steel Bars and Shapes
ASTM A565 Specification for Martensitic Stainless Steel Bars, Forgings, and Forging Stock for High Temperature Service
ASTM A582 Specification for Free Machining Stainless Steel Bars
Tubes & Pipes
ASTM A182 Specification for Forged or Rolled Alloy-Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service
ASTM A268 Specification for Seamless and Welded Ferritic Stainless Steel Tubing for General Service
ASTM A269 Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service
ASTM A312 Seamless and Welded Austenitic Stainless Steel Pipe
ASTM A358 Electric Fusion Welded Austenitic Chromium Nickel Alloy Steel Pipe for High Temperature Service
ASTM A403 Specification for Wrought Austenitic Stainless Steel Piping Fittings
ASTM A409 Specification for Welded Large Diameter Austenitic Steel Pipe for Corrosive or High Temperature Service
ASTM A511 Specification for Seamless Stainless Steel Mechanical Tubing
ASTM A554 Specification for Welded Stainless Steel Mechanical Tubing
ASTM A632 Specification for Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service
ASTM A731 Specification for Seamless and Welded Ferritic Stainless Steel Pipe
ASTM A789 Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Tubing for General Service
ASTM A790 Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe
ASTM A813 Specification for Single or Double Welded Austenitic Stainless Steel Pipe
ASTM A814 Specification for Cold Worked Welded Austenitic Stainless Steel Pipe
Forgings
ASTM A473 Specification for Stainless Steel Forgings
ASTM A705 Specification for Age Hardening Stainless and Heat Resisting Steel Forgings
Castings
ASTM A297 Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat-Resistant for General Application
ASTM A743 Standard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
ASTM A744 Standard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service
ASTM A890 Standard Specification for castings, iron-chromium-nickel-molybdenum corrosion-resistant, duplex (austenitic/ferritic) for general application