Standards, Specifications & Grades
ASTM standards A297, A351, A743, A744 and A890 specify castings for corrosion and heat-resisting service. These include stainless steels and some nickel based alloys. The grade designations used in these standards are those originally developed by the ACI, the Alloy Casting Institute. (Now the Steel Founder’s Society of America). The chemical composition of stainless steel grades covered by these standards include ACI grade designations CA6N CA6NM CA15 CA15M CA28MWV CA40 CA40F CB6 CB30 CB7Cu-1 CB7Cu-2 CC50 CD3MCuN CD3MN CD3MWCuN CD4MCu CD6MN CE20N CE3MN CE30 CE8MN CF3 CF8 CF8C CF20 CF3M CF3MN CF8M CF8C CF10 CF10M CF10MC CF10SMnN CF16F CF16FA CG6MMN CG3M CG8M CG12 CH8 CH10 CH20 CK20 CK3MCuN CK35MN CN3M CN3MN CN7M CN7MSCT15C HC HD HE HF HH HI HK HK30 HK40 HL HN HP HT HT30 HU HW HX. Duplex castings grades 1A 1B 1C 2A 3A4A 5A 6A are also listed and cross references to wrought AISI grades 410 420 304L 304 347 302 316L 316LN 316 317 317L 309 310 made. Common grade names are also cross referenced and include 17/4PH 15/5PH 2205 Zeron 100 Alloy 958 Escoloy 254SMO and AL-6XN
Most ASTM and ASME standards list the steel grades by their UNS (Unified Numbering system) numbers but also make reference, where appropriate to the more general AISI (American Iron and Steel Institute) grade designations. These grade numbering systems are widely used in the USA, where they originated and are recognised by most stainless steel specifiers and users. In Japan the AISI grade number is preceded by SUS eg SUS 304. The chemical compositions of stainless steel grades covered in this article include AISI / common grade names 301 301L 301LN 302 302B 303 XM-5 303Plus X 303Se 303Cu 304 304L 302HQ XM-21 304HN 304LN 305 308 316 316L 316Ti 316Cb316LN 317 317L 317LM 317LMN 317LN 321 347 347F 347FSe 348 384 201 Gall-Tough 202 XM-1 203EZ 205 XM-19 Nitronic 50 XM-31 Tenelon XM-14 XM-17 216 XM-18 216L Nitronic 60 21-6-9 Nitronic 40 XM-11 XM-29 Nitronic 33 18-2Mn Nitronic 32 18-18 Plus 20Cb-3 20Mo-4 20Mo6 Sanicro28 AL-6X AL-6XN JS700 904L 1925hMo Cronifer 1815 LCSi 310MoLN 254SMO 654SMO Nirosta 4565S XM-15 18-8-2 SAE grades 30301 30302 30302B 30303 30303Se 30304 30304L 30305 30308 30316 30316L 30317 30321 30347 30348 30384 30201 30202 and UNS grades S30100 S30103 S30153 S30200 S30215 S30300 S30310 S30323 S30330 S30400 S30403 S30430 S30452 S30453 S30454 S30500 S30800 S31600 S31603 S31635 S31640 S31653 S31700 S31703 S31725 S31726 S31753 S32100 S34700 S34720 S34723 S34800 S38400 S20100 S20103 S20153 S20161 S20162 S20200 S20300 S20400 S20500 S20910 S21400 S21460 S21600 S21603 S21800 S21900 S21904 S24000 S24100 S28200 N08020 N08024 N08026 N08028 N08366 N08367 N08700 N08904 N08925 N08926 S30600 S30601 S31050 S31254 S31266 S31277 S32050 S32615 S32654 S34565 S35135 S38100 S38815
Most ASTM and ASME standards list the steel grades by their UNS (Unified Numbering system) numbers but also make reference, where appropriate to the more general AISI (American Iron and Steel Institute) grade designations. These grade numbering systems are widely used in the USA, where they originated and are recognised by most stainless steel specifiers and users. In Japan the AISI grade number is preceded by SUS, but this is not usually the case with duplex grades. The chemical compositions of stainless steel grades covered in this article include AISI / common grade names XM-26 44LN DP3 3RE60 2205 UR45N 2304 Uranus 50 Uranus 52N+ Ferralium 255 2507 Zeron 100 329 44L 453S 7Mo Plus DP3W AF918 and UNS grades S31100 S31200 S31260 S31500 S31803 S32001 S32003 S32101 S32205 S32304 S32404 S32520 S32550 S32750 S32760 S32900 S32906 S32950 S39226 S39274 S39277
Most ASTM and ASME standards list the steel grades by their UNS (Unified Numbering system) numbers but also make reference, where appropriate to the more general AISI (American Iron and Steel Institute) grade designations. These grade numbering systems are widely used in the USA, where they originated and are recognised by most stainless steel specifiers and users. In Japan the AISI grade number is preceded by SUS eg SUS 430. The chemical compositions of stainless steel grades covered in this article include AISI / common grade names 403 405 409 410S 430 430F 430FSe 434 436 442 XM-34 18-2FM Cronifer 2803Mo 435 439 439LL 444 18Cr-2Mo X-M33 26-1Ti XM-27 NuMonit 25-4-4 Sea-cure 26-3-3 29-4 29-4-2 SAE grades 51403 51405 51409 51430 51430F 51430FSe 51434 51436 51439 51439LL and UNS grades S18200 S18235 S40300 S40500 S40800 S40900 S40910 S40920 S40930 S40945 S40975 S40976 S40977 S41003 S41008 S41045 S41050 S41500 S41603 S42035 S43000 S43020 S43023 S43036 S43400 S43600 S44200 S32803 S43035 S43900 S43903 S43932 S43940 S44400 S44500 S44626 S44627 S44635 S44660 S44700 S44735 S44800 S46800
Most ASTM and ASME standards list the steel grades by their UNS (Unified Numbering system) numbers but also make reference, where appropriate to the more general AISI (American Iron and Steel Institute) grade designations. These grade numbering systems are widely used in the USA, where they originated and are recognised by most stainless steel specifiers and users. In Japan the AISI grade number is preceded by SUH eg SUH 310. The chemical compositions of stainless steel grades covered in this article include AISI / common grade names 304H 304N 304HN (XM-21) 309S 309 309H 309Cb 309HCb 310S 310 310H 310Cb 310HCb 314 316H 316N 321H 334 347H 348 348H 446 616 Esshete 1250 153MA 253MA 353MA RA85H Greek Ascoloy (615) Lapelloy (619) MT443 XM-32 800 (332) 800H SAE grades 30309 30309S 30310 30310S 30314 51446 and UNS grades S21500 S30409 S30415 S30451 S30452 S30615 S30815 S30900 S30908 S30909 S30940 S30941 S31000 S31008 S31009 S31040 S31041 S31400 S31609 S31651 S32109 S33228 S33400 S34709 S34800 S34809 S35045 S35315 S41041 S41425 S41800 S42200 S42300 S44300 S44600 S64152 N08800 N08810 N08811
Most ASTM and ASME standards list the steel grades by their UNS (Unified Numbering system) numbers but also make reference, where appropriate to the more general AISI (American Iron and Steel Institute) grade designations. These grade numbering systems are widely used in the USA, where they originated and are recognised by most stainless steel specifiers and users. In Japan the AISI grade number is preceded by SUS eg SUS 630. The chemical compositions of stainless steel grades covered in this article include AISI / common grade names 410 414 416 416Se 420 420F 420FSe 429 431 440A 440B 440C 440F 440FSe 630 631 632 633 634 635 PH13-8Mo 15-5PH 15-7PH 17-4PH 17-7PH A286 Trim Rite XM-6 (416 Plus X) XM-13 XM-12 XM-16 Custom 455 XM-25 Custom 450 XM-30 SAE grades 51410 51414 51416 51416Se 51420 51420F 51420FSe 51429 51431 51440A 51440B 51440C 51440F 51440FSe and UNS grades S13800 S15500 S15700 S17400 S17600 S17700 S35000 S35500 S41000 S41040 S41400 S41500 S41600 S41610 S41623 S42000 S42010 S42020 S42023 S42900 S43100 S44002 S44003 S44004 S44020 S44023 S45000 S45500 S45503 S46500 S66286
Summary of links to websites for download of stainless steel grade datasheets