10. Stainless Steel Datasheets for Tubular Products

Introduction

The Stainless Steel Advisory Service receives requests for datasheets for individual steel grades. Rather than create a new set of datasheets, it has been decided to make use of the excellent datasheets which already exist. These datasheets are most often linked to BSSA Members. Occasionally, I have included a datasheet for grades which are not covered by Members’ datasheets.

Steel grades are arranged according to the main EN standards for tubular products. The codes used in the following tables are:

Aalco Aalco
AM Aperam
DMV DMV
Out Outokumpu
RA Rolled Alloys
Sand Sandvik

The existence of a datasheet for the more unusual grades probably indicates the ability to supply. However, the Special Grades Matrix gives a more comprehensive list of companies able to supply the product.

 Datasheets for Welded Tubes Based on EN 10296-2 and EN 10217-7

The table below contains all grades listed in EN 10296-2 (welded tubes for general purposes) and EN 10217-7 (welded tubes for pressure purposes).  Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Grades in both standards are shown in bold. Grades only in EN 10296-2 are shown in normal. Grades only in EN 10217-7 are shown in italic.

EN Designation Alternative Designations
Steel name Steel number AISI UNS Other US BS Generic/Brand Datasheets
Ferritic stainless steels
X2CrNi12 1.4003 S40977 3CR12 Aalco AM
X2CrTi12 1.4512 409 S40900 409S19 AM
X6CrAl13 1.4002 405 S40500 405S17
X6Cr17 1.4016 430 S43000 430S17 AM
X3CrTi17 1.4510 439 S43035 AM
X2CrMoTi18-2 1.4521 444 S44400 AM
X6CrMoNb17-1 1.4526 436 S43600 AM
X2CrTiNb18 1.4509 441 S43932 18CrCb AM
Austenitic stainless steels
X2CrNiN18-7 1.4318 301LN S30153
X2CrNi18-9 1.4307 304L S30403   304S11     AM      
X2CrNi19-11 1.4306 304L  S30403         AM      
X2CrNiN18-10 1.4311 304LN  S30453   304S51          
X5CrNi18-10 1.4301 304 S30400   304S15   AM      
X6CrNiTi18-10 1.4541 321  S32100   321S31     AM    
X6CrNiNb18-10 1.4550 347 S34700   347S31        
X2CrNiMo17-12-2 1.4404 316L  S31603   316S11     AM      
X5CrNiMo17-12-2 1.4401 316 S31600   316S31     AM      
X6CrNiMoTi17-12-2 1.4571 316Ti  S31635   320S31     AM      
X2CrNiMo17-12-3 1.4432 316L  S31603   316S13          
X2CrNiMoN17-3-3 1.4429 316LN S31653                
X3CrNiMo17-13-3 1.4436 316 S31600   316S33            
X2CrNiMo18-14-3 1.4435 316L  S31603   316S13        
X2CrNiMoN17-13-5 1.4439 317LMN S31726           But  
X1NiCrMoCu25-20-5 1.4539   N08904    904S13  904L   Outo    
X1CrNiMoCuN20-18-7 1.4547   S31254 F44   254SMO     Outo  
X6CrNiMoNb17-12-2 1.4580 S31640
X2CrNiMo18-15-4 1.4438 317L S31703   317S12          
X1CrNiMoCuN24-22-8 1.4652 S32654 654SMO Outo
X1NiCrMo31-27-4 1.4563   N08028     Sanicro 28       But
X1CrNiMoCuN25-25-5 1.4537 N08932
X1CrNiMoCuNW24-22-6 1.4659 S31266
X1NiCrMoCuN25-20-7 1.4529   N08925     1925hMo       But 
Austenitic stainless steels – heat resisting Grades
X15CrNiSi20-12 1.4828 AM
X9CrNiSiNCe21-11-2 1.4835 S30815 253 MA RA
X12CrNi23-13 1.4833 309 S30900 309S24 AM RA 
X8CrNi25-21 1.4845 310S S31000 310S24 RA
X6CrNiSiNCe19-10 1.4818 S30415 153 MA Outo
X6NiCrSiNCe35-25 1.4854 S35315 353MA
X10NiCrSi35-19 1.4886 N08330 330 RA
Austenitic-ferritic stainless steels
X2CrMnNiN21-5-1 1.4162 S32101 2101 LDX Outo
X2CrNiN23-4 1.4362   S32304     2304     Outo  
X2CrNiMoN12-5-3 1.4462   S31803/

S32205

 F51   2205   Outo RA
X2CrNiMoN25-7-4 1.4410   S32750   F53   2507     Outo    
X2CrNiMoCuEWN25-7-4 1.4501 S32760 F55 Zeron 100 RA

Datasheets for Seamless Tube Products Based on EN 10297-2 and EN 10216-5

The table below contains all grades listed in EN 10297-2 (seamless tubes for general purposes) and EN 10216-5 (seamless tubes for pressure purposes). Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Grades in both standards are shown in bold. Grades only in EN 10297-2 are shown in normal. Grades only in EN 10216-5 are shown in italic.

EN Designation Alternative designation
Steel name Steel number AISI UNS Other US BS Generic/Brand Datasheets
Ferritic stainless steels
X2CrTi12 1.4512 409 S40900 409S19
X6CrAl13 1.4002 405 S40500 405S17
X6Cr17 1.4016 430 S43000 430S17
X3CrTi17 1.4510 439 S43035
Martensitic stainless steels
X12Cr13 1.4006 410 S41000
Austenitic stainless steels
X2CrNi18-9 1.4307 304L S30403   304S11            
X2CrNi19-11 1.4306 304L S30403                
X2CrNiN18-10 1.4311 304LN S30453                
X5CrNi18-10 1.4301 304 S30400   304S31          
X8CrNiS18-9 1.4305 303 S30300 303S31  
X6CrNiTi18-10 1.4541 321 S32100   321S31            
X6CrNiNb18-10 1.4550 347 S34700   347S31            
X1CrNi25-21 1.4335 310L S31002         Sand      
X2CrNiMo17-12-2 1.4404   S31603   316S11             
X5CrMo17-12-2 1.4401 316 S31600   316S31            
X1CrNiMoN25-22-2 1.4466 310MoLN S31050       DMV Sand      
X6CrNiMoTi17-12-2 1.4571 316Ti S31635   320S31            
X6CrNiMoNb17-12-2 1.4580   S31640                
X2CrNiMoN17-13-3 1.4429 316LN S31653                
X3CrNiMo17-13-3 1.4436 316 S31600   316S33          
X2CrNiMo18-14-3 1.4435 316L S31603       DMV Sand      
X2CrNiMoN17-13-5 1.4439   S31703                
X1NiCrMoCu31-27-4 1.4563   N08028     Sanicro 28   Sand      
X1NiCrMoCu25-20-5 1.4539   N08904     904L   Sand      
X1CrNiMoCuN20-18-7 4 1.4547   S31254     254 SMO   Sand      
X1NiCrMoCuN25-20-7 1.4529   N08925                
X2NiCrAlTi32-20 1.4558   N08800         Sand    
Ferritic heat resisting steels
X18CrN28 1.4749 S44600 Sand
Austenitic heat resisting steels
X8CrNiTi18-10 1.4878 321 S32109
X9CrNiSiNCe21-11-2 1.4835 S30815 253 MA Sand
X12CrNi23-13 1.4833 S30900 309S24 Sand
X8CrNi25-21 1.4845 310S S31008 310S31 Sand
X10NiCrAlTi32-21 1.4876 N08810
X6NiCrSiNCe35-25 1.4854 S35315 Sand
X10NiCrSi35-19 1.4886 N08330 330 RA
 Austenitic creep resisting steels
X6CrNi18-10 1.4948 304H
X7CrNiTi18-10 1.4940 321H
X7CrNiNb18-10 1.4912 347H
X6CrNiTiB18-10 1.4941 321H
X6CrNiMo17-13-2 1.4918 316N Sand
X5NiCrAlT31-20 1.4958
X8CrNiAlTi32-21 1.4959 Sand
X3CrNiMoBN17-13-3 1.4910 316LN
X8CrNiNb16-13 1.4961
X8CrNiMoVNb16-13 1.4988
X8CrNiMoNb16-16 1.4981
X10CrNiMoMnNbVB15-10-1 1.4982 Sand
Austenitic-ferritic stainless steels
X2CrNiN23-4 1.4362   S32304     2304   Sand    
X3CrNiMoN27-5-2 1.4460 329 S31260 Sand
X2CrNiMoN29-7-2 4 1.4477
X2CrNiMoN22-5-3 1.4462   S31803/

S32205

    2205 DMV Sand      
X2CrNiMoCuN25-6-3 1.4507   S32550     Ferrinox 255 DMV        
X2CrNiMoN25-7-4 4 1.4410   S32750     2507   Sand    
X2CrNiMoCuWN25-7-4 1.4501   S32760     Zeron 100 DMV        
X2CrNiMoSi18-5-3 1.4424   S31500         Sand      